Magnesium Sacrificial Anodes
-
Magnesium Anodes Cathodic Protection
-
High Potential Magnesium Anode
-
Magnesium Ribbon Anode
-
Extruded Magnesium Anodes
-
Prepackaged Magnesium Anode
-
Water Heater Magnesium Anode
-
Wrought Magnesium Alloy
-
Magnesium Alloy Bar
-
High Strength Magnesium Alloy
-
Magnesium Alloy Sheet
-
Dissolvable Magnesium Alloy
-
Magnesium Rare Earth Alloy
-
FedererReliable quality of sacrificial magnesium anode.
-
AliceWell suited to our cathodic protection needs.
G97 Extruded Hot Water Heater Magnesium Az80 Anode Rod Replacement
Place of Origin | CHINA |
---|---|
Certification | USA: G97,ASTM |
Minimum Order Quantity | 1000KGS |
Price | Negotiable |
Packaging Details | Pallet packing, or on customer's request |
Delivery Time | 30 Days after receiving the deposit |
Payment Terms | 50% Deposit , 50% Balance before deliver to the port |
Supply Ability | 500 mts per month |

Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
xProduct Name | Magnesium Metal Rod Sacrificial Anode | Shape | Rod |
---|---|---|---|
Application | Water Heater | Material | Magnesium Alloy |
Dimensions | Customer's Demands,Many | Chemical Composition | Al,Mn,Zn,Mg |
Standard | High Quality | Color | Silver |
High Light | G97 Extruded Hot Water Heater Magnesium Rod,Hot Water Heater Magnesium Rod Az80,Az80 Anode Rod Replacement |
High Weight Ratio Extruded Magnesium Anodes Widely Used Where Small Anode Diameters
Introduction:
Extruded magnesium anodes have a high surface to length ratio in relation to cross-sectional size. This allows these anodes to provide higher current per unit weight than standard cast magnesium anodes. By supplying more current, extruded anodes can provide effective protection for structures buried in high resistivity soils.
Features:
The extruded magnesium alloy anode rod adopts a continuous drawing production process. The surface of the product is smooth, without pores and slag inclusions, the potential is greater than 1.48V, the efficiency is greater than 55%, and the bar yield is over 98%.
Chemical composition %:
Alloy | Al | Mn |
Zn (max) |
Ca (max) |
Si (max) |
Cu (max) |
Ni (max) |
Fe (max) |
Other Imp | |
each | total | |||||||||
AZ31B | 2.5-3.5 | 0.2-1.0 | 0.6-1.4 | 0.04 | 0.10 | 0.01 | 0.001 | 0.005 | --- | 0.30 |
Mg-Mn | 0.01max | 0.5-1.3 | --- | --- | --- | 0.02 | 0.001 | 0.03 | 0.05 | 0.30 |
Specification:
Diameter (inch) |
Core eccentric (inch) |
Core diameter (inch) |
Straightness (inch/2 ft length) |
Weight (1bs/inch) |
0.675-0.020 | 0.050 | 0.135 | 0.060 | 0.025 |
0.750-0.020 | 1/16 | 0.135 | 0.040 | 0.031 |
0.800-0.020 | 1/16 | 0.135 | 0.040 | 0.035 |
0.840-0.020 | 1/16 | 0.135 | 0.040 | 0.038 |
0.900-0.020 | 1/16 | 0.135 | 0.040 | 0.043 |
1.050-0.020 | 1/16 | 0.135 | 0.040 | 0.057 |
1.315-0.020 | 1/16 | 0.135 | 0.040 | 0.089 |
Process flow:
1. Ore smelting (crude magnesium)
2. During the refining process of crude magnesium refining (magnesium ingot), the components are tested by the spectrometer in order to meet the national standard. The samples are reserved for two years for quality traceability.
3. Magnesium ingot casting rod (in the casting rod process, use the spectrometer to test the composition again, and record the furnace number for subsequent quality tracking)
4. Extrusion (the composition of the extrusion process remains unchanged)
5. Cut
6. Packaging
7. Shipping
Application:
Magnesium rod is the common name of magnesium anode, also known as anode magnesium block, which is used to prevent corrosion of metal liner and soften water quality of magnesium rod. In the use of Taigang type or manganese steel metal liner, the principle of electrochemical anti-corrosion sacrificial anode protection of metal in water is used to protect the cathode, the magnesium rod is used as the anode, and the metal liner is used as the cathode. When the enamel coating on the surface of the metal liner is complete, the enamel shields the metal liner, the insulation resistance between the magnesium rod and the metal liner can reach more than 2MΩ, and the output current of the magnesium (rod) anode is almost zero. However, when cracks appear in the enamel liner, a small resistance is formed between the magnesium anode and the metal liner through water, and the magnesium anode starts to output current, which flows to the exposed metal liner to produce a polarized film, which repairs the damage. The enamel, which insulates the inner tank of Jinyu, prevents corrosion.
Photos: